Main > Acta Optica Sinica >  Volume 34 >  Issue 1 >  Page 116002 > Article
  • Abstract
  • Abstract
  • View Summary
  • Figures (0)
  • Tables (0)
  • Equations (0)
  • References (19)
  • Get PDF(in Chinese)
  • Paper Information
  • Received: Jul. 18, 2013

    Accepted: --

    Posted: Jan. 1, 2014

    Published Online: Jan. 2, 2014

    The Author Email: Fen Zhao (416644511@qq.com)

    DOI: 10.3788/aos201434.0116002

  • Get Citation
  • Copy Citation Text

    Zhao Fen, Feng Wenlin, Cheng Xueling. Study on Synthesis and Luminescent Properties of a Novel Orange SrMoO4:Pr3+,B3+,Li+ Phosphor[J]. Acta Optica Sinica, 2014, 34(1): 116002

    Download Citation

  • Category
  • Materials
  • Share
Acta Optica Sinica, Vol. 34, Issue 1, 116002 (2014)

Study on Synthesis and Luminescent Properties of a Novel Orange SrMoO4:Pr3+,B3+,Li+ Phosphor

Fen Zhao1,*, Wenlin Feng1,2, and Xueling Cheng1

Author Affiliations

  • 1[in Chinese]
  • 2[in Chinese]

Abstract

A novel orange SrMoO4:Pr3+, B3+, Li+ phosphor is prepared via the high-temperature solid state reaction process, and its structure, morphology and luminescence properties are studied. The X-ray diffraction (XRD) patterns show that a pure SrMoO4 crytal phase is obtained at 1200 ℃. The morphology of the sample under scanning electron microscope (SEM) has good dispersity and irregular shapes. The excitation spectra are made up of charge transfer band and characteristic transitions of 3H4→3P2,1,0 (448, 473, 487 nm, respectively) of Pr3+. The emission spectra of the SrMoO4:Pr3+, B3+, Li+ phosphors are characterized by peaks at 529(3P1→3H4,5), 545(3P0→3H5), 553(3P0→3H5), 600(1D2→3H4), 617(3P0→3H6), 645 nm (3P0→3F2). The strongest one appears at 645 nm. The intensity of excitation and emission peaks of SrMoO4:Pr3+ can be improved by doping B3+ and Li+. The optimum doping mole fractions are 0.15% B3+ and 0.35% Li+, respectively.